Laser vat exposure and resin removal
A laser cures the photopolymer layer by layer. Plan liquid drainage and cleaning access for hollow bodies and blind channels before building.
Use SLA for fine geometry, assembly checks and appearance prototypes. Select the resin, post-cure and finish around the surfaces that need to fit or stay clear.
Send a STEP/STP model with critical dimensions, the target color or clarity and any areas to mask. Larger one-piece builds need an orientation and distortion review.
Review the print and cleaning, how the resin will be post-cured, and which surfaces must be polished or painted.
A laser cures the photopolymer layer by layer. Plan liquid drainage and cleaning access for hollow bodies and blind channels before building.
Use the approved cure cycle for the resin. Specify reamed holes and inserts separately, with bore size, remaining wall and the installation method for the cured material.
Polish accessible clear surfaces and evaluate a compatible clear coat when specified. For paint, agree a color and gloss sample and identify surfaces to mask.
| Process routes | When to consider it | What to verify | Typical production lead time |
|---|---|---|---|
| Standard cleaned and post-cured finish | Functional prototypes and assembly checks | Print dimensions, fit and allowed support marks | 2–4 business days |
| Cosmetic sanding and PU/UV paint | Show models, finished enclosures and color samples | Color, gloss, film thickness and masked interfaces | 4–6 business days |
| Clear polishing and optional clear coat | Viewing windows, flow models and light guides | Clarity sample, access for polishing and scratch limits | 4–6 business days |
Match each validation task to the resin and define the finished features to inspect.
Evaluate WaterShed XC 11122 for viewing flow. Check resin drainage, the accessible polish area and the required clarity, and specify any leak test separately.
Evaluate ceramic-filled Somos PerFORM where stiffness and heat response matter. Verify the cure, load, temperature and exposure period for the test setup.
Evaluate Somos Taurus for repeated assembly. Set snap deflection, insert installation and pull-out or torque checks around the boss geometry.
Mark the A-surfaces, viewing areas and critical holes on the drawing.
Review thin walls for warping after cure. Place drain and vent openings where resin can flow out and the cavity can be washed and inspected. Size them for the cavity and resin.
Keep support contacts away from viewing, sealing and mating surfaces where possible. Agree where sanding or visible marks are allowed and whether the surface is accessible for polishing.
A 0.04–0.08 mm film per side changes the final fit. If equally coated on opposite faces, an outside diameter grows by 0.08–0.16 mm. Agree mask boundaries or post-finish reaming for close fits.
Choose up to two grades to compare. Send both as alternatives or specify a single grade in the inquiry.
Scroll the table to see the data and applications.
| Resin grade | Material family | Tensile data · ASTM D638 | HDT · 0.455–0.46 MPa | Typical applications |
|---|---|---|---|---|
| Tough charcoal resin | 46.9 MPa (at yield, UV post-cure) · 49 MPa (at yield, thermal post-cure) | 62 °C (UV post-cure) · 91 °C (thermal post-cure) | Snap-fits and functional housings | |
| White ABS-like resin | 56.8 MPa (at yield) | 52 °C (UV post-cure) | Fine-detail housings and painted prototypes | |
| Clear resin | 50.4 MPa (at break, UV post-cure) | 50 °C (UV post-cure) | Viewing windows and fluid paths | |
| Ceramic-filled resin | 68 MPa (UV post-cure) · 80 MPa (thermal post-cure) | 132 °C (UV post-cure) · 268 °C (thermal post-cure) | Stiff tooling and test models | |
| Tough clear photopolymer | 52 ± 3 MPa (at break, post-processed) | 53 °C (post-processed) | Clear guards and flexing parts | |
| Tough black LCD photopolymer | 39–42 MPa (at break, post-processed) | 60–62 °C (post-processed) | Fixtures, black housings and covers |
Typical data are from the manufacturers. Confirm the resin, color, printer and cure for the part. HDT is measured under load and does not define continuous service temperature. Review LOCTITE grades on a validated photopolymer platform.
Manufacturer data sheets · Stratasys · Somos · Somos PerFORM · LOCTITE 3D IND405 · LOCTITE 3D PRO476
Select a grade in the table to start comparing.
Confirm the exact grade, color and platform during engineering review.
Review geometry in the as-printed state and check critical interfaces after the agreed finish.
| Item | Capability and conditions |
|---|---|
| Materials by process | Somos Taurus / EvoLVe 128 / WaterShed XC 11122 / PerFORM · Loctite 3D IND405 / PRO476 |
| One-piece build envelope | 800 × 800 × 550 mm · 1,500 × 750 × 550 mm |
| Layer thickness | 0.05–0.10 mm |
| Typical as-built linear tolerance | ±0.10 mm (≤100 mm) / ±0.15% |
| Selected features after secondary work | ±0.03–0.05 mm |
| Minimum wall, through hole and channel | 0.8–1.0 mm · Ø0.8–1.0 mm · 0.6–0.8 mm |
The first volume is standard. WaterShed is a transparent photopolymer. PerFORM is ceramic-filled. Review supports, post-cure and local reaming separately.
| Item | Capability and conditions |
|---|---|
| SLA/PolyJet finishing and coating | 400–2,000 · PU / UV · 0.04–0.08 mm · ASTM D3359 4B–5B |
| Single-side change after blasting or smoothing | 0.02–0.04 mm |
For adhesion testing on resin, agree the tape-test method, coating sample and rating in advance. ASTM D3359
Agree critical dimensions, reference samples and areas that need scratch protection for shipping.
Check warping and the position of critical holes after cure or secondary work. Agree the datum setup and first-article report scope.
Use the agreed measurement method for coating thickness and compare color and gloss to the reference. Inspect clear faces under the agreed lighting and viewing conditions.
Wrap clear or glossy faces in a suitable non-abrasive layer. Use fitted supports to prevent direct contact and movement during transit.
Specify the resin, finish and secondary operations. Attach the brief with any notes about color, clarity or fit.
The clear finish requires a clear grade. Confirm which of the selected resins should be used for the transparent area.
Your choices and entered requirements will appear here.
For a viewing window or flow model, agree an appearance sample and the surfaces that can be polished. Imaging optics need their own requirements for transmission, haze and surface geometry.
Uncured resin can remain trapped in a closed cavity. Drain and vent openings let it flow out and provide access for cleaning and inspection. Placement depends on orientation and geometry.
Select the resin and cure for the load, temperature and exposure duration. Assess humidity, UV exposure and coating durability for outdoor use. Request service-specific validation if those conditions are critical.