Skip to content

Precision electroplating services

Specify a finish for corrosion protection, electrical contact or appearance. We review the substrate and finish together with critical dimensions, masking and measurement, for supplied parts or a coordinated machining and plating order.

10–25 μmElectroless nickel on carbon/alloy steel
8–12 μmElectroplated zinc on carbon steel
ASTM B568XRF thickness measurement where suitable

Choose the coating by function

Start with the working surface, base alloy and finish required by the drawing. Define the layers separately where they have different functions.

Corrosion protection and wear resistance

Review electroless nickel for machined features, zinc for carbon steel and hard chrome for selected wear surfaces. On deep bores, specify the minimum thickness and the point to check.

Electrical contacts and solderable finishes

Specify gold or silver for the required contact or RF surface, or tin for the specified soldering interface. Control the underplate, contact zone, finish and test method for the application.

Decorative plating and hardware finishes

Review bright nickel–chromium or black nickel against a physical sample. Specify gloss, visible faces and allowed rack marks. For prolonged skin contact, confirm the applicable nickel-release requirements for the finished article.

Plating thickness and specification matrix

The figures apply to the named substrate and layer stack. Other combinations, coating class, hardness and corrosion tests are confirmed against the drawing.

CoatingThickness or review scopeSpecification referenceSubstrate and acceptanceContact and CAD files
Electroless nickel (ENP)10–25 μmASTM B733 Carbon or alloy steel reference. Confirm phosphorus class, heat treatment and significant surfaces.
Zinc electroplating8–12 μmASTM B633 Carbon-steel parts. Specify the passivation or seal, appearance and corrosion acceptance.
Tin electroplating5–10 μmASTM B545 Copper or copper-alloy parts. Agree finish and solderability requirements.
Gold electroplating0.5–2.0 μmNickel underplate 3–5 μmASTM B488 Copper-based contacts. Confirm the contact area, gold type and nickel underplate separately.
Silver electroplating3–8 μmNickel underplate 3–5 μmASTM B700 Copper-based conductive surfaces. Agree the silver zone, underplate and any tarnish protection.
Electroplated nickelAgree on drawingASTM B689 Confirm the purpose, layer stack and substrate-specific activation. Brightness follows the approved finish.
Engineering hard chromeAgree on drawingASTM B177/B177M Selected wear surfaces and fits. Plan grinding allowance and the final dimensional check with the coating.
Decorative nickel / trivalent chromeAgree on drawingASTM B456 Confirm the base and undercoat, trivalent chemistry where requested, gloss and reference sample.
Black nickel / gunmetalAgree on drawingApproved physical sampleConfirm shade, gloss, underlying layers, any seal and wear acceptance.

Substrate preparation and the right fixture

Base metal and activation

Aluminum 6061 / 7075 / 5052
Review cleaning, desmutting and zincate activation for the actual alloy when required by the coating system.
Stainless steel 304 / 316 / 316L / 17-4PH
Identify the exact grade and finish. Review oxide removal and the need for an activation or strike layer.
Carbon and alloy steels
Specify grade, hardness and heat-treated condition. For high-strength parts, agree hydrogen embrittlement controls and any applicable test before releasing the process.
Copper and copper alloys
Review cleaning and activation for the specific alloy. Agree nickel or another specified underplate and any selective coating boundary.

Rack or barrel plating

Rack plating
Review for larger, shaped or appearance-sensitive parts. Agree contact points, allowed rack marks, drainage and masked features.
Barrel plating
Review for small parts that can tumble in bulk. Validate part-to-part contact, tangling, nested shapes and any coating required inside recesses.

Masking, dimensions and coating inspection

Protect bores, threads and contact surfaces

Mark the plating and masking boundaries on the drawing. If a smooth bore is coated on both sides, its diameter decreases by about twice the coating thickness. Review thread geometry separately and verify it with agreed gauges after plating.

Thickness, adhesion and corrosion checks

Review XRF when the layers and measuring locations are suitable. Specify thickness by layer, measurement points and sampling. Agree the adhesion method, specimen and salt spray duration and acceptance criteria when needed.

Dimensional inspection illustration

Protect the finish from inspection to delivery

Separate plated contacts and cosmetic parts so they do not rub together. For silver, agree compatible anti-tarnish materials. Specify ESD packaging only where the product requires it, and link the agreed reports to the lot.

FAQs

How does plating change a close fit?

Define which dimensions apply before and after plating. For bearing seats and threads, agree masking, pre-plate allowance or finish machining and plan the final measurement.

Can machining or fabrication and plating be quoted together?

Yes. Identify the intended finish, key interfaces and final acceptance in one drawing package. For supplied parts, tell us the exact alloy, prior surface treatment and present condition.

Can XRF verify thickness inside every bore?

XRF depends on layer composition, accessible geometry and calibration. Agree significant points and an alternate method, such as a section measurement when needed.

What should I specify for wearable hardware?

Provide the use conditions, physical finish sample and applicable market requirements. For prolonged skin contact, arrange any nickel-release testing on the finished article.

ECHA · REACH Annex XVII, Entry 27

Send drawings and plating requirements

Provide substrate grade, quantity, layer thickness, masked areas and final fit. Name the standard and revision, and include any inspection, sample or compliance requirements.

Plating review brief

Coatings to review

Example for copper contacts: specify the base alloy, nickel underplate and gold layer separately.

Choose a coating or describe your part to request a recommendation.

Contact and CAD files

Drawings & reference files

STEP/STP, PDF, JPG or PNG. Up to 3 files; 10 MB each, 20 MB total.

No files selected

    No drawing yet? Describe the part and application below.

    KEEPWIN · LANGUAGE

    Choose your language

    Select the language you prefer for your visit.

    You can change your language anytime in the menu.